The natural malachite sample used in the study was obtained from Lupe mine, Puebla, Mexico. The sample was crushed, hand-sorted to get lump of malachite for contact …
Flotation experiments showed that LA had a significantly promoting effect on malachite sulfidization flotation. Adsorption experiments and SEM-EDS results indicated that LA improved the adsorption of S (II) species …
Notably, malachite with ammonium sulfide ions had a significantly higher flotation recovery than malachite with an excess of sodium sulfide ions, as concerns of sulfidization types.
The conventional flotation on malachite involves sulphidizing the malachite surface prior to selective flotation using a sulphodryl collector such as xanthate [7]. This process is …
In this study, the effect of the dissolved components derived from malachite and calcite on the flotation behavior and surface characteristics of both minerals was investigated.
At pH 6.50, with 8 mg/L SDA, effectively recovering malachite from quartz was achieved by reverse flotation, in which 92.71% of malachite was recovered and 91.91% of quartz was removed, coupled ...
We study the effects of the growth phase of Rhodococcus opacus on the floatability of malachite. We find that bacteria in stationary phase show more than two-fold …
The majority of reagents currently used in mineral flotation processes are fossil-based and potentially harmful to the environment. Therefore, it is necessary to find …
The flotation performance of malachite was examined through flotation tests conducted using the XFG-II flotation machine located in Jilin, China. The flotation tank had a …
Flotation was first performed in 1860 (Arbiter, 2000) and is a technology that utilizes the differences in physicochemical properties of various mineral surfaces to achieve specific …
Flotation experiments were conducted on a synthetic malachite ore prepared by mixing 10 g malachite with 90 g quartz. All flotation tests were carried out using a 1.5 L Denver …
A wide range of organic polymers are utilized in the mineral industry as flotation agents, serving specific modifying roles like depressants, dispersants, or flocculants …
But during sulfidization flotation, malachite gets . depressed after the add ition of excess sod ium sulfide. So ammonium sulfate, (NH 4) 2 SO 4 is used as a . sulfidization prom oter. [36]
The natural malachite has been ground in the agate mortar till 2-10 m m; part of the sample obtained is used to draw the spectres I.R.; some part of the sample is treated with solution of …
The single mineral flotation results indicate that it may be possible to separate malachite from calcite by sulfidization-xanthate flotation. Hence we test the separation …
Materials. The XRD of malachite, quartz, and calcite were shown in Figure 1.The element analysis of malachite, quartz, and calcite were listed in Table 1. −75 + 38 μm fractions …
In the flotation of malachite, the most widely used method is to use xanthate collectors to float malachite minerals in the presence of sulfidizing reagents, viz. sulfidization …
A natural malachite sample was obtained from the Lupe mine, Puebla, Mexico. The sample was crushed, hand-sorted and dry-ground to obtain different fractions for different …
However, as the oxygen flow rate increased from 0 to 10 sccm, the surface roughness decreased to 0.32 nm, corresponding to an increase in the contact angle to 147 •, …
With the depletion of copper sulfide minerals, malachite has attracted increasing interest. Since malachite is a relatively soft mineral, with a Moh's hardness of 3.5–4 [], fines …
While for malachite, its flotation recoveries increased from 38.26% to 78.62%, and then to 79.41% with nitrogen flow rate increasing from 50 to 200 mL·min −1, and then to 250 …
The flotation results indicate that the PX dosage is a key factor determining the flotation separation results of malachite and calcite. When its dosage reaches 1000 mg/L, the …
Furthermore, the activity of the sulfidization products on the sulfidized mineral surface increased and sulfidization flotation of malachite was promoted. The surface of …
The effects of the bacterial growth phase on the malachite flotation were investigated in a well-controlled Hallimond tube system. Rhodococcus opacus, which is one of …
EPA was first introduced in the lead-free malachite flotation. EPA owned a stronger affinity with malachite, which could enhance its recovery. The corrosive effect caused …
Hydrodynamics factors which contr ibute to the kinetics of flotation such as agitation, air flow rate, ... "Hydroxamate flotation of malachite," Canadia Metal lurgical . Quarterly, no. …
In this study, the flotation behavior of malachite was investigated using carboxyl-functionalized carbon black nanoparticles (CB-NPs) as collectors in a hydrodynamically …
Why LA was first introduced as a sulfidization activator to enhance sulfidization flotation of malachite? Because of its structure? What might be the interaction? What is the …
Copper oxide ores, including malachite [Cu 2 (CO 3)(OH) 2], are indeed essential sources of industrial copper.These ores undergo several techniques to extract copper from the ore, …